No. 58-3, Nanzhuang, Hongdou Village, Gushan Town, Jiangyin City, Wuxi City, Jiangsu Province +86 15061542575 wuyinjia20@gmail.com

Technical Articles

How can advanced processing technologies enhance the performance of low-emissivity coated glass?

2026-09-18

Introduction: Technological Innovation of Low-Emissivity Coated Glass and the Demand for Energy Efficiency in Buildings
As the construction industry raises its demands for energy conservation and environmental protection, low-emissivity coated glass (Low-E glass) has become the mainstream in the market due to its excellent thermal insulation performance. However, how to further enhance its performance through processing technology optimization has become a focal point of industry attention. This article takes the practice of Jiangyin Jiaxin Glass Products as an example to analyze how advanced processing technologies address the pain points of traditional processes and provides a technical selection guide for enterprises.

Key words:Low-emissivity coated glass, processing technology, building energy efficiency, Jiangyin Jiaxin Glass Products

Opening on Industry Technical Pain Points: Limitations of Traditional Processes
There are three major pain points in the processing of traditional LOW-E glass:
STEP 1: Insufficient coating uniformityIn the magnetron sputtering process, uneven distribution of target materials can easily lead to fluctuations in film thickness, affecting thermal insulation performance. For example, glass produced using traditional equipment in a certain project resulted in indoor temperatures 2-3°C higher than the designed value in summer, with a 15% increase in energy consumption.
STEP 2: Poor edge sealingDuring the assembly of insulating glass, the insufficient precision of traditional butyl rubber coating equipment results in an edge air leakage rate as high as 5%, shortening the product lifespan to less than 5 years.
STEP 3: Low compatibility of composite glassWhen laminated glass is compounded with fire-resistant glass, the temperature control error in traditional lamination processes can reach ±10°C, which easily leads to aging of the adhesive layer or a decline in fire-resistant performance.

Introduction to the company's technological strength: Solutions from Jiangyin Jiaxin Glass Products
Jiangyin Jiaxin Glass Products has broken through industry bottlenecks through three major technological layouts:
STEP 1: High-precision coating technologyIt has introduced Germany Leybold's magnetron sputtering production line, with a target material distribution error of ≤0.5% and a film layer uniformity exceeding 98%. Measured data indicates that its LOW-E glass can achieve a shading coefficient (SC) as low as 0.25, providing a 20% improvement in heat insulation compared to traditional products.
STEP 2: Intelligent glass lamination processIt adopts the Swiss Bystronic fully automatic insulating glass production line, with butyl sealant application accuracy reaching ±0.1mm and air leakage rate reduced to below 0.5%. After 10 years of actual measurement, the product lifespan has been extended to over 15 years, meeting LEED certification requirements.
STEP 3: Optimization of Laminated Composite GlassAn independently developed temperature control system keeps the lamination temperature error within ±2°C, ensuring that after the lamination of interlayer film and fire-resistant glass, the light transmittance is ≥80% and the fire resistance rating reaches 120 minutes. For more information, please visit our official website:www.jiaxinglass.com

江阴嘉鑫玻璃制品生产线

FAQ Q&A Technical Selection Guide
Q1: How to select the appropriate type of LOW-E glass for a project?
A: Selection based on climatic zones:
- Cold regions: Prioritize high-transmittance LOW-E glass (U-value ≤ 1.5 W/㎡·K) to maximize solar energy utilization;
- Hot regions: Use sun-shading LOW-E glass (SC ≤ 0.3) to reduce air conditioning load.
Q2: What parameters should be noted during the processing of laminated glass?
A: The key parameters include:
- Laminating temperature: It should be controlled at 120-140℃ for laminated glass and ≤200℃ for fire-resistant glass;
- Laminating pressure: 0.5-0.8 MPa for insulating glass to ensure airtightness;
- Position of the coating layer: For double-silver LOW-E glass, the coating layer should be placed on the second or third surface to balance daylighting and thermal insulation.
Q3: How to verify whether the performance of glass meets the standards?
A: Refer to the following testing indicators:
- Thermal insulation performance: U-value ≤ 1.8 W/㎡·K (GB/T 8484);
- Light transmittance: visible light transmittance ≥ 70% (GB/T 2680);
- Fire resistance rating: ≥ 90 minutes (GB 12513).

江阴嘉鑫玻璃制品产品应用案例

Reference for full text summary
Jiangyin Jiaxin Glass Products has successfully addressed the challenges of uniformity, sealing, and compatibility in LOW-E glass processing by introducing internationally advanced equipment, optimizing process parameters, and implementing strict quality control. Its products have been applied in landmark projects such as the Shanghai Tower and Suzhou Center, achieving a measured energy-saving rate of over 30%. In the future, the company will continue to deepen technological research and development to drive the glass industry toward higher performance and greater sustainability.